{"id":1528,"date":"2025-12-23T10:37:08","date_gmt":"2025-12-23T10:37:08","guid":{"rendered":"https:\/\/citations.tools.bio-logic.fr\/?p=1528"},"modified":"2025-12-23T10:37:08","modified_gmt":"2025-12-23T10:37:08","slug":"properties-of-coatings-created-by-hvof-technology-using-micro-and-nano-sized-powder","status":"publish","type":"post","link":"https:\/\/citations.tools.bio-logic.fr\/?p=1528","title":{"rendered":"Properties of coatings created by HVOF technology using micro-and nano-sized powder"},"content":{"rendered":"<h4>DOI:<\/h4>\n<p><a href=\"https:\/\/doi.org\/10.2478\/kom-2019-0011\" target=\"_blank\" rel=\"noopener\">10.2478\/kom-2019-0011<\/a><\/p>\n<h4>Authors:<\/h4>\n<p>Anna Guzanov\u00e1, Janette Brezinov\u00e1, Dagmar Draganovsk\u00e1, Pavlo Maruschak<\/p>\n<h4>Abstract:<\/h4>\n<p>Abstract The paper focuses on assessment the resistance of hot-sprayed coatings applied by HVOF technology (WC\u2013Co\u2013Cr created using powder of two different grain sizes) against erosive wear by dry-pot wear test in a pin mill at two sample angles. As these coatings are designated for the environment with varying elevated temperatures and often are in contact with the abrasive, the coatings have been subjected to thermal cyclic loading and their erosive resistance has been determined in as-sprayed condition and after the 5 th and 10th thermal cycles. The corrosion resistance of coatings was evaluated by linear polarization (Tafel analysis).<\/p>\n","protected":false},"excerpt":{"rendered":"<h4>DOI:<\/h4>\n<div class=\"b-doi\">10.2478\/kom-2019-0011<\/div>\n<h4>Authors:<\/h4>\n<div class=\"b-author\">Anna Guzanov\u00e1, Janette Brezinov\u00e1, Dagmar Draganovsk\u00e1, Pavlo Maruschak<\/div>\n<h4>Abstract:<\/h4>\n<div class=\"b-intro\">Abstract The paper focuses on assessment the resistance of hot-sprayed coatings applied by HVOF technology (WC\u2013Co\u2013Cr created using powder of two different grain sizes) against erosive wear by dry-pot wear test in a pin mill at two sample angles. As these coatings are designated for the environment with varying elevated&hellip;<\/div>\n","protected":false},"author":1,"featured_media":0,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[25],"tags":[37],"class_list":["post-1528","post","type-post","status-publish","format-standard","hentry","category-sp-150-potentiostat","tag-corrosion"],"_links":{"self":[{"href":"https:\/\/citations.tools.bio-logic.fr\/index.php?rest_route=\/wp\/v2\/posts\/1528","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/citations.tools.bio-logic.fr\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/citations.tools.bio-logic.fr\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/citations.tools.bio-logic.fr\/index.php?rest_route=\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/citations.tools.bio-logic.fr\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=1528"}],"version-history":[{"count":0,"href":"https:\/\/citations.tools.bio-logic.fr\/index.php?rest_route=\/wp\/v2\/posts\/1528\/revisions"}],"wp:attachment":[{"href":"https:\/\/citations.tools.bio-logic.fr\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=1528"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/citations.tools.bio-logic.fr\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=1528"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/citations.tools.bio-logic.fr\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=1528"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}